Rubber-weiss plasticity testing machine TRWM-A10 the pressurized heavy hammer slides moves in up and down axial direction to measure the deformation occurred due to heavy pressure hammer displacement. 3 minutes after completion of the test, clock stops automatically, bringing hammer back to normal position. The dial indicator fixed on the top bracket of TRWM-A10 measures the sample deformation caused by heavy pressure hammer displacement.
A (1 to 6) J indicating error ± 0.05 J
B (1 to 12) J indicating error ± 0.05 J
C (1 to 24) J indicating error ± 0.05 J
D (1 to 48) J indicating error ± 0.05 J
The indicating errors w.r.t measurement range of 20 to 80 %
Frictional resistance
Pyramid dimension
Three sides: 60×60×60 mm, height 25 ± 0.7 mm, Arris edge fillet radius 1.5 ± 0.1 mm